Quote:
Originally Posted by sqcomp
It doesn't take much...just doing. 500 ml of resin, use maybe 5 cc's of MEKp type stuff. Instead of cutting your mat rip it so that you have frayed ends so that they blend better. Little things like this. It's been a few years since I did this so I wasted around 1000 mL of resin from making it too hot with hardener. You should have seen my first try! The damn resin was smoking. It actually singed the cardboard that was in the trash can. No $hit.
|
Bout 8 years ago I was glassing in the middle of winter... it was 20F outside, I had to use enough MEKp to make it smoke just to ensure the stuff got hot enough to cure. I had a few spots that didn't get hot enough, and they stayed goey for like two months. Since then i've decided not to glass anytime is below 40F.